In this guide · 5 practical sections

Dye stage, dye system and wash effect are separate
Garment dyeing means the garment is sewn before colouring. Reactive and pigment refer to different colour systems. Acid wash is a trade name for a mottled finish; it is not a specification for which chemicals a laundry must use.
How each garment process works
| Process | Short production sequence | Typical appearance | What to approve |
|---|---|---|---|
| Piece dyeing | The fabric is dyed before cutting and sewing. | A more uniform base is often the target. | Check roll shade, usable width and cutting-lot separation. |
| Reactive garment dye | A suitable sewn garment is prepared, dyed, then washed off, dried and checked. | Colour on compatible cellulosic components; trims or seams may contrast. | Trial thread, rib, elastane, trims and measurements after processing. |
| Pigment garment dye | A compatible garment is prepared, colour is deposited with a binder system, then the finish is set and checked. | Surface-led colour and a worn-in effect, depending on the process. | Assess dry/wet crocking, seam highlights, hand feel and ageing. |
| Acid wash / mottled fade | The laundry develops uneven fading on a suitable sewn garment, then stops the process, rinses and checks the finished piece. | Clouding or irregular highlights. The trade name does not specify a chemical recipe. | Approve an acceptable visual range and check strength, shade variation, staining and dimensions. |
| Enzyme wash | The laundry applies an enzyme process suitable for the substrate, then stops it and rinses. | May soften the surface or reduce surface fuzz; outcome depends on material. | Check hand feel, weight change, colour and strength as relevant. |
| Stone or mechanical wash | Controlled agitation or abrasion creates wear effects; the garment is then cleaned and inspected. | Texture and seam-edge highlights. | Check seam wear, holes, damage to trims and lot consistency. |
| Softener / finishing wash | A compatible wash and finishing treatment adjusts handle or appearance. | A softer or different drape, with limited or no intended fading. | Review finish durability, shade and compatibility with print and function. |
A practical approval sequence
- Agree the base fabric, thread, rib, trims and an approved visual reference.
- Make a sewn test garment. Confirm whether branding should be applied before or after wet processing.
- Have the professional laundry run a pilot, rinse, dry and condition the garment before checking it.
- Approve a light-to-dark range as well as the target, and record measurements, staining and performance before releasing bulk.
Example: for a washed charcoal hoodie, compare the body and rib in the same light; look for excessive contrast at seams, trim damage and unacceptable mottling. Check chest, length and sleeve after finishing, then confirm rub fastness and care performance on the approved finish.
Related guides and tools
Technical references
Questions, answered
What is the difference between garment dye and acid wash?
Garment dye applies colour after sewing. Acid wash is a trade name for an irregular faded look. A laundry can evaluate a suitable base and route on a pilot garment.
Can I get exactly the same acid-wash pattern on every hoodie?
Mottled effects naturally vary. Approve reference samples at the light and dark ends of the acceptable range, and check how contrast looks on the body, rib and seams.
Should printing happen before or after garment washing?
It depends on the look and durability requirement. Test the actual decoration and wash order on sewn samples and approve the one that meets the specification.